Serial number | Project | Detail |
1 | Camera light source | HD line scan camera; Line laser |
2 | Size |
1.Specific combination of actual layout scheme design 2.Automatic blanking is provided |
3 | Capacity | >4000 |
4 | Support cell |
1. Single crystal 2. 156-230mm |
5 | Cell state | Finished battery piece shoot the front of the battery piece |
6 | Shooting defect |
PL can be photographed defects: black spots suction cup marks graphite boats hidden cracks etching oil spots concentric circles scratches Other pollution and all the usual defects(★Different battery processes will lead to differences in the strength of defect imaging) |
7 | Process contribution |
1.AI algorithm automatically detects 2.Hidden crack culling alarm to prevent batch defects 3.Break grid virtual printing alarm prevent batch defects |
8 | Advantage |
1.Contactless loss 2.Probe free loss 3.High productivity 4.SE offset off grid virtual printing poor sintering appear white more obvious than EL |